-40%

MIG Welding Wire ER308L Stainless Steel .035" 2.5Lb (1)

$ 10.02

Availability: 100 in stock
  • Welding Wire Material: Stainless Steel
  • All returns accepted: ReturnsNotAccepted
  • Country/Region of Manufacture: United States
  • Condition: Total 2.5lbs (1) one
  • Diameter: 0.035 in
  • Brand: Sandvik
  • Roll Weight: 2.5 lb

    Description

    SANDVIK MIG Welding Wire ER308L Stainless Steel .035"
    2.5Lb x 1 Roll
    2.5 Lb Total
    Fast shipping USPS
    Class:
    ER308L
    AWS:
    A5.9
    Conforms to Certification: AWS A5.9           ASME SFA A5.9
    Weld Process Used for Mig (GMAW) and Submerged Arc (SAW)
    AWS Chemical Composition
    C = 0.03 max
    Cr = 19.5-22.0
    Ni = 9.0 – 11.0
    Mo = 0.75 max
    Mn = 1.0 – 2.5
    Si = 0.30 – 0.65
    P = 0.03 max
    S = 0.03 max
    Cu = 0.75 max
    Available Sizes
    Diameter X Spool Sizes
    Diameter X Coil Sizes
    .025 x 2#, 10#, 25#
    1/16 x 60# & mill coil
    .030 x 2#, 10#, 25#, 30#, 33#
    5/64 x 60# & mill coil
    .035 x 2#, 10#, 25#, 30#, 33#
    3/32 x 60# & mill coil
    .045 x 2#, 10#, 25#, 30#, 33#
    1/8 x 60# & mill coil
    1/16 x 10#, 25#, 30#, 33#
    3/16 x 60# & mill coil
    5/32 x 60# & mill coil
    Application
    ER308L has the same analysis as type 308 except the carbon content has been held to a maximum of .03% to reduce the possibility of intergranular carbide precipitation. ER308L is ideal for welding Types 304L, 321, and 347 stainless steels. This is a suitable wire for applications at cryogenic temperatures.
    Deposited Chemical Composition % (Typical)
    C = 0.02
    Si = 0.32
    Mn = 1.70
    P = 0.011
    S = 0.009
    Cr = 20.0
    Ni = 10
    Mechanical Properties (R.T.)
    Yield Strength
    57,000 psi
    Tensile Strength
    87,000 psi
    Elongation
    34%
    Reduction of Area
    56%
    Deposited All Weld Metal Properties
    Data is typical for ER308L weld metal deposited by Mig using Argon + 2% oxygen as the shielding gas. Data on sub-arc is not presented, as sub-arc is dependent on the type of flux used.
    Recommended Welding Parameters
    GMAW “Mig Process”
    Reversed Polarity
    Wire Diameter
    Wire Feed
    Amps
    Volts
    Shielding Gas
    Gas CFH
    Short Arc Welding
    .030
    13-26
    40-120
    16-20
    Argon+2% O2
    25
    .035
    13-26
    60-140
    16-22
    Argon+2% O2
    25
    Spray Arc Welding
    .035
    20-39
    140-220
    24-29
    Argon+2% O2
    38
    .045
    16-30
    160-260
    25-30
    Argon+2% O2
    38
    1/16
    10-16
    230-350
    27-31
    Argon+2% O2
    38
    Other shielding Gases may be used for Mig welding. Shielding gases are chosen taking Quality, Cost, and Operability into consideration
    Recommended Welding Parameters
    SAW “Submerged Arc Welding Process”
    Reversed Polarity Suggested
    Wire Diameter
    Amps
    Volts
    3/32
    250-450
    28-32
    1/8
    300-500
    29-34
    5/32
    400-600
    30-35
    3/16
    500-700
    30-35
    Both Agglomerated and fused fluxes can be used for submerged arc welding.